Owing to high specific energy, low cost, and environmental friendliness, lithium–sulfur (Li–S) batteries hold great promise to meet the increasing demand for advanced energy storage beyond portable ...electronics, and to mitigate environmental problems. However, the application of Li–S batteries is challenged by several obstacles, including their short life and low sulfur utilization, which become more serious when sulfur loading is increased to the practically accepted level above 3–5 mg cm−2. More and more efforts have been made recently to overcome the barriers toward commercially viable Li–S batteries with a high sulfur loading. This review highlights the recent progress in high‐sulfur‐loading Li–S batteries enabled by hierarchical design principles at multiscale. Particularly, basic insights into the interfacial reactions, strategies for mesoscale assembly, unique architectures, and configurational innovation in the cathode, anode, and separator are under specific concerns. Hierarchy in the multiscale design is proposed to guide the future development of high‐sulfur‐loading Li–S batteries.
High‐sulfur‐loading lithium–sulfur (Li–S) batteries enabled by multiscale hierarchical design principles are reviewed. The basic insights into the interfacial reactions, strategies for mesoscale assembly, unique architectures, and configurational innovation in the cathode, anode, and separator are of specific concern. Hierarchy in the multiscale design is proposed to guide the future development of high‐sulfur‐loading Li–S batteries.
Full text
Available for:
FZAB, GIS, IJS, KILJ, NLZOH, NUK, OILJ, SAZU, SBCE, SBMB, UL, UM, UPUK
Lithium (Li) metal has been considered as an important substitute for the graphite anode to further boost the energy density of Li‐ion batteries. However, Li dendrite growth during Li ...plating/stripping causes safety concern and poor lifespan of Li metal batteries (LMB). Herein, fluoroethylene carbonate (FEC) additives are used to form a LiF‐rich solid electrolyte interphase (SEI). The FEC‐induced SEI layer is compact and stable, and thus beneficial to obtain a uniform morphology of Li deposits. This uniform and dendrite‐free morphology renders a significantly improved Coulombic efficiency of 98% within 100 cycles in a Li | Cu half‐cell. When the FEC‐protected Li metal anode matches a high‐loading LiNi0.5Co0.2Mn0.3O2 (NMC) cathode (12 mg cm−2), a high initial capacity of 154 mAh g−1 (1.9 mAh cm−2) at 180.0 mA g−1 is obtained. This LMB with conversion‐type Li metal anode and intercalation‐type NMC cathode affords an emerging energy storage system to probe the energy chemistry of Li metal protection and demonstrates the material engineering of batteries with very high energy density.
Fluoroethylene carbonate (FEC) additive is used to form a LiF‐rich solid electrolyte interphase (SEI). The FEC‐induced SEI layer is compact and stable, and therefore beneficial to obtain a uniform morphology of Li deposits. When the FEC‐protected Li metal anode matches a high‐loading oxide cathode, a high initial capacity and stable cycling are achieved.
Full text
Available for:
BFBNIB, FZAB, GIS, IJS, KILJ, NLZOH, NUK, OILJ, SAZU, SBCE, SBMB, UL, UM, UPUK
Practical application of lithium (Li) metal anodes has been hindered by Li dendrite growth, which renders a low Coulombic efficiency and short lifespan of working Li metal batteries. A stable solid ...electrolyte interphase (SEI) is crucial in suppressing the formation of Li dendrites. Herein the local stress and deformation evolvement status of a SEI layer during Li electrodeposition are investigated through a quantitative electrochemical–mechanical model based on a finite element method. Furthermore, the impacts of structural uniformity and mechanical strength on the stability of the SEI under different working conditions are investigated. Improving the structural uniformity of SEI is the most effective way to enhance the stability of SEI, which regulates ion transportation. In addition, pursuing extremely high mechanical strength is shown to be pointless, and a moderate elastic modulus of 3.0 GPa is suggested. This work affords an insight into the rational design of stable SEI layers and sheds light on a possible pathway toward practical applications of Li metal anodes.
The failure mechanism of a solid electrolyte interphase (SEI) is systematically studied based on a quantitative electrochemical–mechanical model. How the SEI regulates Li dendrite growth, when SEI fails, and what is the key determinant for stable SEIs are discussed in detail. This work affords theoretical guidance for the design of stable SEIs.
Full text
Available for:
FZAB, GIS, IJS, KILJ, NLZOH, NUK, OILJ, SAZU, SBCE, SBMB, UL, UM, UPUK
Sluggish reaction kinetics and severe shuttling effect of lithium polysulfides seriously hinder the development of lithium‐sulfur batteries. Heterostructures, due to unique properties, have ...congenital advantages that are difficult to be achieved by single‐component materials in regulating lithium polysulfides by efficient catalysis and strong adsorption to solve the problems of poor reaction kinetics and serious shuttling effect of lithium‐sulfur batteries. In this review, the principles of heterostructures expediting lithium polysulfides conversion and anchoring lithium polysulfides are detailedly analyzed, and the application of heterostructures as sulfur host, interlayer, and separator modifier to improve the performance of lithium‐sulfur batteries is systematically reviewed. Finally, the problems that need to be solved in the future study and application of heterostructures in lithium‐sulfur batteries are prospected. This review will provide a valuable reference for the development of heterostructures in advanced lithium‐sulfur batteries.
Heterostructures could regulate lithium polysulfides by efficient catalysis and strong adsorption to solve the problems of poor reaction kinetics and serious shuttling effect of lithium‐sulfur batteries. This review systematically and detailedly analyzes the principle and the application of heterostructures as sulfur host, interlayer, and separator modifier to promote the performance of lithium‐sulfur batteries.
Full text
Available for:
BFBNIB, FZAB, GIS, IJS, KILJ, NLZOH, NUK, OILJ, SAZU, SBCE, SBMB, UL, UM, UPUK
Safe and rechargeable lithium metal batteries have been difficult to achieve because of the formation of lithium dendrites. Herein an emerging electrolyte based on a simple solvation strategy is ...proposed for highly stable lithium metal anodes in both coin and pouch cells. Fluoroethylene carbonate (FEC) and lithium nitrate (LiNO3) were concurrently introduced into an electrolyte, thus altering the solvation sheath of lithium ions, and forming a uniform solid electrolyte interphase (SEI), with an abundance of LiF and LiNxOy on a working lithium metal anode with dendrite‐free lithium deposition. Ultrahigh Coulombic efficiency (99.96 %) and long lifespans (1000 cycles) were achieved when the FEC/LiNO3 electrolyte was applied in working batteries. The solvation chemistry of electrolyte was further explored by molecular dynamics simulations and first‐principles calculations. This work provides insight into understanding the critical role of the solvation of lithium ions in forming the SEI and delivering an effective route to optimize electrolytes for safe lithium metal batteries.
Not dead ′Li′: Fluoroethylene carbonate (FEC) and lithium nitrate (LiNO3) were concurrently introduced into an electrolyte, thus altering the solvation sheath of lithium ions and forming a uniform solid electrolyte interphase (SEI). An abundance of LiF and LiNxOy is formed on the working lithium metal anode and contributes to dendrite‐free lithium deposition.
Full text
Available for:
BFBNIB, FZAB, GIS, IJS, KILJ, NLZOH, NUK, OILJ, SAZU, SBCE, SBMB, UL, UM, UPUK
The lithium metal battery is strongly considered to be one of the most promising candidates for high-energy-density energy storage devices in our modern and technology-based society. However, ...uncontrollable lithium dendrite growth induces poor cycling efficiency and severe safety concerns, dragging lithium metal batteries out of practical applications. This review presents a comprehensive overview of the lithium metal anode and its dendritic lithium growth. First, the working principles and technical challenges of a lithium metal anode are underscored. Specific attention is paid to the mechanistic understandings and quantitative models for solid electrolyte interphase (SEI) formation, lithium dendrite nucleation, and growth. On the basis of previous theoretical understanding and analysis, recently proposed strategies to suppress dendrite growth of lithium metal anode and some other metal anodes are reviewed. A section dedicated to the potential of full-cell lithium metal batteries for practical applications is included. A general conclusion and a perspective on the current limitations and recommended future research directions of lithium metal batteries are presented. The review concludes with an attempt at summarizing the theoretical and experimental achievements in lithium metal anodes and endeavors to realize the practical applications of lithium metal batteries.
Full text
Available for:
IJS, KILJ, NUK, PNG, UL, UM
Solid‐state lithium (Li) metal batteries (SSLMBs) have become a research hotspot in the energy storage field due to the much‐enhanced safety and high energy density. However, the SSLMBs suffer from ...failures including dendrite‐induced short circuits and contact‐loss‐induced high impedance, which are highly related to the Li plating/stripping kinetics and hinder the practical application of SSLMBs. The maximum endurable current density of lithium battery cycling without cell failure in SSLMB is generally defined as critical current density (CCD). Therefore, CCD is an important parameter for the application of SSLMBs, which can help to determine the rate‐determining steps of Li kinetics in solid‐state batteries. Herein, the theoretical and practical meanings for CCD from the fundamental thermodynamic and kinetic principles, failure mechanisms, CCD identifications, and influence factors for improving CCD performances are systematically reviewed. Based on these fundamental understandings, a series of strategies and outlooks for future researches on SSLMB are presented, endeavoring on increasing CCD for practical SSLMBs.
The critical current density (CCD) is an important standard for future solid‐state Li metal batteries (SSLMBs), which is highly related to power density and fast charge capability. The CCD can help to unravel the rate determining factors of Li kinetics including special mass transport and charge transfer at solid–solid interfaces.
Full text
Available for:
BFBNIB, FZAB, GIS, IJS, KILJ, NLZOH, NUK, OILJ, SAZU, SBCE, SBMB, UL, UM, UPUK
Lithium metal battery has been considered as one of the potential candidates for next‐generation energy storage systems. However, the dendrite growth issue in Li anodes results in low practical ...energy density, short lifespan, and poor safety performance. The strategies in suppressing Li dendrite growth are mostly conducted in materials‐level coin cells, while their validity in device‐level pouch cells is still under debate. It is imperative to address dendrite issues in pouch cells to realize the practical application of Li metal batteries. This review presents a comprehensive overview of the failure mechanism and regulation strategies of Li metal anodes in practical pouch cells. First, the gaps between the scientific findings in materials‐level coin cells and device‐level pouch cells are underscored. Specific attention is paid to the mechanistic understanding and quantitative discussion on the failure mechanisms of pouch‐type Li metal batteries. Subsequently, recently proposed strategies are reviewed to suppress dendrite growth in pouch cells. The state‐of‐the‐art electrochemical performance of pouch cells, especially the cell‐level energy density and lifespan, is critically concerned. The review concludes with an attempt to summarize the scientific and engineering understandings of pouch‐type Li metal anodes and propose some novel insights for the practical applications of Li metal batteries.
This review presents a comprehensive overview of the gaps between the materials‐level coin cells and device‐level pouch cells, mechanistic understanding and quantitative discussion for failure mechanisms of pouch‐type Li metal anodes, and the recently proposed strategies to suppress dendrite growth in pouch cells.
Full text
Available for:
FZAB, GIS, IJS, KILJ, NLZOH, NUK, OILJ, SAZU, SBCE, SBMB, UL, UM, UPUK
Lithium (Li) metal is the most promising electrode for next‐generation rechargeable batteries. However, the challenges induced by Li dendrites on a working Li metal anode hinder the practical ...applications of Li metal batteries. Herein, nitrogen (N) doped graphene was adopted as the Li plating matrix to regulate Li metal nucleation and suppress dendrite growth. The N‐containing functional groups, such as pyridinic and pyrrolic nitrogen in the N‐doped graphene, are lithiophilic, which guide the metallic Li nucleation causing the metal to distribute uniformly on the anode surface. As a result, the N‐doped graphene modified Li metal anode exhibits a dendrite‐free morphology during repeated Li plating and demonstrates a high Coulombic efficiency of 98 % for near 200 cycles.
The matrix: Nitrogen‐doped graphene is used as the Li plating matrix to regulate Li metal nucleation and suppress dendrite growth. The N‐containing functional groups in the N‐doped graphene are lithiophilic, which guide the Li nucleation and give a uniform distribution of Li on the anode surface. The dendrite‐free lithium‐metal anodes exhibit an impressive electrochemical performance.
Full text
Available for:
BFBNIB, FZAB, GIS, IJS, KILJ, NLZOH, NUK, OILJ, SAZU, SBCE, SBMB, UL, UM, UPUK
The lithium metal anode is regarded as a promising candidate in next‐generation energy storage devices. Lithium nitrate (LiNO3) is widely applied as an effective additive in ether electrolyte to ...increase the interfacial stability in batteries containing lithium metal anodes. However, because of its poor solubility LiNO3 is rarely utilized in the high‐voltage window provided by carbonate electrolyte. Dissolution of LiNO3 in carbonate electrolyte is realized through an effective solvation regulation strategy. LiNO3 can be directly dissolved in an ethylene carbonate/diethyl carbonate electrolyte mixture by adding trace amounts of copper fluoride as a dissolution promoter. LiNO3 protects the Li metal anode in a working high‐voltage Li metal battery. When a LiNi0.80Co0.15Al0.05O2 cathode is paired with a Li metal anode, an extraordinary capacity retention of 53 % is achieved after 300 cycles (13 % after 200 cycles for LiNO3‐free electrolyte) and a very high average Coulombic efficiency above 99.5 % is achieved at 0.5 C. The solvation chemistry of LiNO3‐containing carbonate electrolyte may sustain high‐voltage Li metal anodes operating in corrosive carbonate electrolytes.
Liquid assets: LiNO3 can be dissolved directly in an ethylene carbonate/diethyl carbonate electrolyte mixture by adding a trace amount of copper fluoride to promote dissolution. The solvation structure of the electrolyte system protects the lithium metal anode in a working high‐voltage lithium metal battery. NCA=LiNi0.80Co0.15Al0.05O2.
Full text
Available for:
BFBNIB, FZAB, GIS, IJS, KILJ, NLZOH, NUK, OILJ, SAZU, SBCE, SBMB, UL, UM, UPUK