E-viri
Recenzirano
-
Kachanov, V. K.; Sokolov, I. V.; Matyunin, V. M.; Barat, V. A.; Bardakov, V. V.; Marchenkov, A. Yu
Measurement techniques, 10/2017, Letnik: 60, Številka: 7Journal Article
The possibility of the effective use of the kinetic indentation method in combination with the acoustic emission method for evaluating the fracture toughness of titanium nitride hardening coatings is shown. It is established that the occurrence of the first jog on the loading line of the kinetic indentation diagram in “load–indentor displacement–time” coordinates is due to the formation of the first crack in the coating and practically coincides in time with the occurrence of the acoustic emission impulse with an increased energy value. This permits a more accurate and substantiated determination of the critical load, indentation depth of the indentor, and hardness at which the first visible ring crack forms around the impression on the coating surface.
![loading ... loading ...](themes/default/img/ajax-loading.gif)
Vnos na polico
Trajna povezava
- URL:
Faktor vpliva
Dostop do baze podatkov JCR je dovoljen samo uporabnikom iz Slovenije. Vaš trenutni IP-naslov ni na seznamu dovoljenih za dostop, zato je potrebna avtentikacija z ustreznim računom AAI.
Leto | Faktor vpliva | Izdaja | Kategorija | Razvrstitev | ||||
---|---|---|---|---|---|---|---|---|
JCR | SNIP | JCR | SNIP | JCR | SNIP | JCR | SNIP |
Baze podatkov, v katerih je revija indeksirana
Ime baze podatkov | Področje | Leto |
---|
Povezave do osebnih bibliografij avtorjev | Povezave do podatkov o raziskovalcih v sistemu SICRIS |
---|
Vir: Osebne bibliografije
in: SICRIS
To gradivo vam je dostopno v celotnem besedilu. Če kljub temu želite naročiti gradivo, kliknite gumb Nadaljuj.